Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Q65B Polyurethane Rubber

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Q65B Polyurethane Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resistance and tensile strength, with fluid compatibility approaching that of NBR. Polyurethane seals provide outstanding performance in hydraulic systems, which are prone to abrasive contamination and high shock loads. Good resistance to weathering and ozone but poor against water and high temperature.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
75
75
°IRHD, +15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 16.8 MPa
2440 psi
-20% change after 70 hours @ 100°C; ASTM D412
21.0 MPa
3050 psi
ASTM D412
Elongation at Break 210 %
210 %
-40% change after 70 hours @ 100°C; ASTM D412
350 %
350 %
ASTM D412
Compression Set 25 %
25 %
70 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
-30.0 °C
-22.0 °F
Flash Point >= 204 °C
>= 399 °F
Users viewing this material also viewed the following: