Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V60H Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V60H Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fluoroelastomer Rubber, 60 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA). Water and n-Hexane extraction tested in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600. ASTM designation = FKM. ISO designation = FPM.Applications: Excellent oil and heat resistance. For repeated use in equipment associated with the production of foodstuffs intended for human consumption. For use with aqueous or fatty foods.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
70
70
°IRHD, +10 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 7.50 MPa
1090 psi
-25% change after 72 hours @ 250°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 150 %
150 %
-25% change after 72 hours @ 250°C; ASTM D412
200 %
200 %
ASTM D412
Compression Set 30 %
30 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Descriptive Properties Value Comments
Extraction Test, 21 CFR 177.2600 pass
Distilled Water
pass
n-Hexane
Users viewing this material also viewed the following: