Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer
Manufacturer Proto3000
Trade Name Objet Digital Materials™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the desired mechanical properties and to resemble the product’s target materials.Information provided by Proto3000 for their protoyping engineering services.
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 - 40.0 MPa
4350 - 5800 psi
ASTM D638-03
Elongation at Break 40 - 50 %
40 - 50 %
ASTM D638-05
Modulus of Elasticity 1.20 - 1.60 GPa
174 - 232 ksi
ASTM D638-04
Flexural Strength 40.0 - 50.0 MPa
5800 - 7250 psi
ASTM D790-03
Flexural Modulus 1.30 - 1.70 GPa
189 - 247 ksi
ASTM D790-04
Izod Impact, Notched 0.350 - 0.450 J/cm
0.656 - 0.843 ft-lb/in
ASTM D256-06
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06