| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
| Water Absorption | 0.30 % | 0.30 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | 1.5 % | 1.5 % | Immersion; ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell E | 66 | 66 | ASTM D785 |
| Hardness, Rockwell M | 107 | 107 | ASTM D785 |
| Hardness, Shore D | 90 | 90 | ASTM D2240 |
| Tensile Strength | 62.1 MPa | 9000 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 3.96 GPa | 575 ksi | ASTM D638 |
| Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
| Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
| Compressive Strength | 138 MPa | 20000 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 2.41 GPa | 350 ksi | ASTM D695 |
| Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 Type A |
| Coefficient of Friction, Dynamic | 0.20 | 0.20 | Dry vs. Steel; QTM55007 |
| K (wear) Factor | 635 x 10<sup>-8</sup> mm³/N-M | 315 x 10<sup>-10</sup> in³-min/ft-lb-hr | QTM 55010 |
| Limiting Pressure Velocity | 0.263 MPa-m/sec | 7500 psi-ft/min | 4:1 safety factor; QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 36.0 µm/m-°C @Temperature -40.0 - 149 °C |
20.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
| Thermal Conductivity | 0.405 W/m-K | 2.81 BTU-in/hr-ft²-°F | ASTM E 1530-11 |
| Maximum Service Temperature, Air | 260 °C | 500 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
| Glass Transition Temp, Tg | 275 °C | 527 °F | ASTM D3418 |
| Flammability, UL94 | V-0 | V-0 | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Limited | Limited | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Limited | Limited | |
| Chlorinated Solvents | Acceptable | Acceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Acceptable | Acceptable | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Machinability | 6 | 1-10, 1=Easier to Machine |