| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | Qualchem Zrt. |
| Trade Name | Danamid |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Qualchem Danamid AFES-21 Polyamide 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | DIN 53479 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527-1,2 |
| Elongation at Yield | 4.0 % | 4.0 % | ISO 527-1,2 |
| Tensile Modulus | >= 3.59 GPa | >= 521 ksi | ISO 527-1,2 |
| Flexural Strength | 82.0 MPa | 11900 psi | 10 mm/min; DIN 53452 |
| Flexural Modulus | 2.07 GPa | 300 ksi | DIN 53452 |
| Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
| 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180 | |
| Izod Impact, Unnotched (ISO) | NB | NB | ISO 180 |
| NB @Temperature -23.0 °C |
NB @Temperature -9.40 °F |
ISO 180 | |
| Charpy Impact Unnotched | NB @Temperature -20.0 °C |
NB @Temperature -4.00 °F |
DIN 53453 |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DIN 53453 | |
| Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 187 °C | 369 °F | DIN 53461 |
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | DIN 53461 |
| Flammability, UL94 | HB @Thickness 4.00 mm |
HB @Thickness 0.157 in |
MSZ 10383 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | DIN 53482 |
| Comparative Tracking Index | 400 V | 400 V | IEC 112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | 2.0 - 2.2 % | 2.0 - 2.2 % | DIN 53714 |