Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quantum Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Quantum Advanced Engineering Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Quantum Advanced Engineering Plastics
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 1.2 %
1.2 %
ASTM D570
Water Absorption at Saturation 8.5 %
8.5 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Tensile Modulus 2.83 GPa
410 ksi
ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 2.76 GPa
401 ksi
ASTM D790
Compressive Strength 86.2 MPa
12500 psi
ASTM D695
Compressive Modulus 2.90 GPa
420 ksi
ASTM D695
Shear Strength 68.9 MPa
10000 psi
ASTM D732
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Coefficient of Friction 0.25
0.25
Thermal Properties Metric English Comments
CTE, linear 72.0 - 79.2 µm/m-°C
40.0 - 44.0 µin/in-°F
ASTM D696
Thermal Conductivity 0.245 W/m-K
1.70 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 260 °C
500 °F
ASTM D3417
Maximum Service Temperature, Air 104 °C
220 °F
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
425 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.7 °C
197 °F
ASTM D648
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.030

@Frequency 1.00e+6 Hz
0.030

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
FDA Compliance yes
Users viewing this material also viewed the following: