| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
| Water Absorption | 0.10 % | 0.10 % | ASTM D570 |
| Water Absorption at Saturation | 0.50 % | 0.50 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 110 | 110 | ASTM D785 |
| Hardness, Rockwell R | 126 | 126 | ASTM D785 |
| Hardness, Shore D | 87 | 87 | ASTM 2240 |
| Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
| Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
| Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
| Compressive Strength | 117 MPa | 17000 psi | ASTM D695 |
| Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
| Shear Strength | 53.1 MPa | 7700 psi | ASTM D732 |
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
| Coefficient of Friction | 0.40 | 0.40 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
| Thermal Conductivity | 0.251 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 332 °C | 630 °F | ASTM D3417 |
| Maximum Service Temperature, Air | 249 °C | 480 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.3 @Frequency 1.00e+6 Hz |
3.3 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 18.9 kV/mm | 480 kV/in | ASTM D149 |
| Dissipation Factor | 0.0030 @Frequency 1.00e+6 Hz |
0.0030 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FDA Compliance | yes |