| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized |
| Manufacturer | Ravago Manufacturing Americas, LLC |
| Trade Name | Hylon® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ravago Manufacturing Americas Hylon® N2017STHL Nylon 6 (DAM).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
| Water Absorption | 1.0 % | 1.0 % | 24 hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | 0.125 in; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
| Elongation at Break | 3.5 % | 3.5 % | ASTM D638 |
| Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
| Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | 73°F; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 39.6 µm/m-°C @Temperature 20.0 °C |
22.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
| Drying Temperature | 73.9 °C | 165 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Moisture Content | 0.18 % | 0.18 % | |
| Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
| Screw Speed | 50 - 120 rpm | 50 - 120 rpm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure | 750 to 1400 psi | |
| Injection Rate | Fast |