Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Physical Properties Metric English Comments
Viscosity 2400 cP
2400 cP
Mechanical Properties Metric English Comments
Adhesive Bond Strength 17.0 MPa
2470 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Descriptive Properties Value Comments
Color Black