| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP LUBRICOMP |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.940 % | 0.940 % | 50% RH, 24 hrs; ASTM D570 |
| 1.18 % | 1.18 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D955 |
| 0.0223 cm/cm @Time 86400 sec |
0.0223 in/in @Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.0259 cm/cm @Time 86400 sec |
0.0259 in/in @Time 24.0 hour |
ISO 294 |
| 0.026 cm/cm @Time 86400 sec |
0.026 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 73.0 MPa | 10600 psi | ISO 527 |
| 74.0 MPa | 10700 psi | ASTM D638 | |
| Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527 |
| 75.0 MPa | 10900 psi | ASTM D638 | |
| Elongation at Break | 14.3 % | 14.3 % | ASTM D638 |
| 17.6 % | 17.6 % | ISO 527 | |
| Elongation at Yield | 13.5 % | 13.5 % | ASTM D638 |
| 16.7 % | 16.7 % | ISO 527 | |
| Tensile Modulus | 3.08 GPa | 447 ksi | 50 mm/min; ASTM D638 |
| 3.17 GPa | 460 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
| 112 MPa | 16200 psi | ASTM D790 | |
| Flexural Modulus | 2.84 GPa | 412 ksi | ISO 178 |
| 3.04 GPa | 441 ksi | ASTM D790 | |
| Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 8.97 J/cm | 16.8 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 59.0 kJ/m² | 28.1 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
| Coefficient of Friction, Dynamic | 0.27 | 0.27 | ASTM D3702 Modified |
| Coefficient of Friction, Static | 0.23 | 0.23 | ASTM D3702 Modified |
| K (wear) Factor | 98.7 x 10<sup>-8</sup> mm³/N-M | 49.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 82.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 82.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 85.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 85.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 74.0 °C | 165 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 76.0 °C @Thickness 3.20 mm |
169 °F @Thickness 0.126 in |
unannealed; ASTM D648 |