| Category | Polymer , Thermoplastic , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP LUBRICOMP |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
| 1.05 g/cc | 0.0379 lb/in³ | ASTM D 792 | |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D 955 |
| 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D 955 |
| 0.0061 cm/cm @Time 86400 sec |
0.0061 in/in @Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 527 |
| 28.0 MPa | 4060 psi | ASTM D 638 | |
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D 638 |
| 37.0 MPa | 5370 psi | ISO 527 | |
| Elongation at Break | 4.8 % | 4.8 % | ASTM D 638 |
| 9.3 % | 9.3 % | ISO 527 | |
| Elongation at Yield | 1.3 % | 1.3 % | ASTM D 638 |
| 1.3 % | 1.3 % | ISO 527 | |
| Tensile Modulus | 3.02 GPa | 438 ksi | 1 mm/min; ISO 527 |
| 3.44 GPa | 499 ksi | 50 mm/min; ASTM D 638 | |
| Flexural Strength | 41.0 MPa | 5950 psi | ASTM D 790 |
| 60.0 MPa | 8700 psi | ISO 178 | |
| Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D 790 |
| 3.10 GPa | 450 ksi | ISO 178 | |
| Izod Impact, Notched | 0.100 J/cm @Temperature 23.0 °C |
0.187 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| Izod Impact, Unnotched | 0.960 J/cm @Temperature 23.0 °C |
1.80 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
| Izod Impact, Notched (ISO) | 2.00 kJ/m² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
| Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
| Coefficient of Friction, Dynamic | 0.23 | 0.23 | ASTM D 3702 Modified |
| Coefficient of Friction, Static | 0.15 | 0.15 | ASTM D 3702 Modified |
| K (wear) Factor | 10930 x 10<sup>-8</sup> mm³/N-M | 5425 x 10<sup>-10</sup> in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 74.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 88.0 °C | 190 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 88.0 °C @Thickness 3.20 mm |
190 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 80.0 °C @Thickness 3.20 mm |
176 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |