Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ISO 1183
0.976 g/cc
0.0353 lb/in³
ASTM D792
Moisture Absorption 0.0200 %
0.0200 %
50% RH, 24 hrs; ASTM D570
0.0200 %
0.0200 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow >= 0.020 cm/cm

@Time 86400 sec
>= 0.020 in/in

@Time 24.0 hour
ASTM D955
>= 0.020 cm/cm

@Time 86400 sec
>= 0.020 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
14.0 MPa
2030 psi
ISO 527
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
23.0 MPa
3340 psi
ISO 527
Elongation at Break 43.2 %
43.2 %
ASTM D638
82.8 %
82.8 %
ISO 527
Elongation at Yield 14 %
14 %
ISO 527
15.8 %
15.8 %
ASTM D638
Tensile Modulus 0.870 GPa
126 ksi
1 mm/min; ISO 527
1.07 GPa
155 ksi
50 mm/min; ASTM D638
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
27.0 MPa
3920 psi
ISO 178
Flexural Modulus 0.870 GPa
126 ksi
ASTM D790
0.930 GPa
135 ksi
ISO 178
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 63.0 J
46.5 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
46.0 °C

@Thickness 3.20 mm
115 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm - 1e+05
100 ohm-cm - 1e+05
ASTM D257
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257