| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP STAT-KON |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | ASTM D792 |
| 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.500 % | 0.500 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Time 86400 sec |
0.0025 in/in @Time 24.0 hour |
ISO 294 |
| 0.0030 cm/cm @Time 86400 sec |
0.0030 in/in @Time 24.0 hour |
ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Time 86400 sec |
0.011 in/in @Time 24.0 hour |
ASTM D955 |
| 0.011 cm/cm @Time 86400 sec |
0.011 in/in @Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 173 MPa | 25100 psi | ASTM D638 |
| 207 MPa | 30000 psi | ISO 527 | |
| Tensile Strength, Yield | 173 MPa | 25100 psi | ASTM D638 |
| 207 MPa | 30000 psi | ISO 527 | |
| Elongation at Break | 1.8 % | 1.8 % | ASTM D638 |
| 2.6 % | 2.6 % | ISO 527 | |
| Elongation at Yield | 1.8 % | 1.8 % | ASTM D638 |
| 2.6 % | 2.6 % | ISO 527 | |
| Tensile Modulus | 14.36 GPa | 2083 ksi | 1 mm/min; ISO 527 |
| 15.16 GPa | 2199 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 282 MPa | 40900 psi | ASTM D790 |
| 361 MPa | 52400 psi | ISO 178 | |
| Flexural Modulus | 11.03 GPa | 1600 ksi | ASTM D790 |
| 17.0 GPa | 2470 ksi | ISO 178 | |
| Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 62.0 kJ/m² | 29.5 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 21.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 21.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 201 °C | 394 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 262 °C @Thickness 3.20 mm |
504 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 249 °C | 480 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 253 °C @Thickness 3.20 mm |
487 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1e+05 - 1.00e+10 ohm | 1e+05 - 1.00e+10 ohm | ASTM D257 |