| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
| 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.140 % | 0.140 % | 50% RH, 24 hrs; ASTM D570 |
| 0.210 % | 0.210 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.00040 - 0.0010 cm/cm @Time 86400 sec |
0.00040 - 0.0010 in/in @Time 24.0 hour |
ASTM D955 |
| 0.00040 - 0.0013 cm/cm @Time 86400 sec |
0.00040 - 0.0013 in/in @Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
| 0.0035 - 0.0040 cm/cm @Time 86400 sec |
0.0035 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 148 MPa | 21500 psi | ISO 527 |
| 150 MPa | 21800 psi | ASTM D638 | |
| Elongation at Break | 1.8 % | 1.8 % | ISO 527 |
| 1.9 % | 1.9 % | ASTM D638 | |
| Tensile Modulus | 16.7 GPa | 2420 ksi | 1 mm/min; ISO 527 |
| 19.58 GPa | 2840 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
| 226 MPa | 32800 psi | ISO 178 | |
| Flexural Modulus | 14.54 GPa | 2109 ksi | ASTM D790 |
| 16.5 GPa | 2390 ksi | ISO 178 | |
| Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 9.00 J | 6.64 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 27.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 27.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 27.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 27.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.5 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 141 °C @Thickness 3.20 mm |
286 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |