Material Notes:
LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
1.23 g/cc
0.0444 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.00080 cm/cm

@Time 86400 sec
0.00080 in/in

@Time 24.0 hour
ISO 294
0.0010 cm/cm

@Time 86400 sec
0.0010 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
0.0032 cm/cm

@Time 86400 sec
0.0032 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 119 MPa
17300 psi
ASTM D638
127 MPa
18400 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
2.6 %
2.6 %
ASTM D638
Tensile Modulus 9.55 GPa
1390 ksi
50 mm/min; ASTM D638
10.12 GPa
1468 ksi
1 mm/min; ISO 527
Flexural Strength 179 MPa
26000 psi
ASTM D790
187 MPa
27100 psi
ISO 178
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
8.25 GPa
1200 ksi
ISO 178
Izod Impact, Notched 2.08 J/cm
3.90 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 J
7.38 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 46.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
46.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 82.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
82.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
327 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
157 °C

@Thickness 3.20 mm
315 °F

@Thickness 0.126 in
unannealed; ASTM D648