| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP VERTON |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
| Water Absorption | 0.90 % <br>@Time 86400 sec |
0.90 % <br>@Time 24.0 hour |
ISO 62-1 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm <br>@Time 86400 sec |
0.0030 in/in <br>@Time 24.0 hour |
ISO 294 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm <br>@Time 86400 sec |
0.0080 in/in <br>@Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
| Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
| Elongation at Break | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
| 3.0 % | 3.0 % | Flexural Strain, break, 2 mm/min; ISO 178 | |
| Elongation at Yield | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 17.8 GPa | 2580 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 366 MPa | 53100 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 15.0 GPa | 2180 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 498 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| Deflection Temperature at 1.8 MPa (264 psi) | 256 °C | 493 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
| UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
| UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
| Flammability, UL94 | HB <br>@Thickness 0.750 mm |
HB <br>@Thickness 0.0295 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Wire Ignition, HWI | 0.00 - 2.0 sec | 0.00 - 2.0 sec | UL 746A |
| High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |