Shakespeare Isocor™ HW69SI Nylon 610

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer Shakespeare Company
Trade Name Isocor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Isocor™ HW69SI Nylon 610.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Isocor™ HW69SI is a medium viscosity PA-610. This resin is specifically suited for applications requiring low moisture absorption and greater dimensional stability. Isocor™ HW69SI is also used in applications requiring good electrical insulation properties. This resin can be processed using conventional techniques. Used for cable jacketing, monofilaments / bristles, film extrusions, electrical connectors, and automotive tubing.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D 638
Elongation at Break 100 %
100 %
ASTM D 638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D 790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D 256
Taber Abrasion, mg/1000 Cycles 6.0
6.0
ASTM D 1044
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D 648