Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Sika Industry
Trade Name SikaFlex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sika Industry SikaFlex 255FC Fast Cure One Part Polyurethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Sika 255FC SikaFlex Fast Cure One Part Polyurethane AdhesiveThis is a fast curing flexible high performance polyurethane adhesive for bonding glass to metal surfaces. Initial strength is derived from its high viscosity. It offers extremely high initial bond strength. It has excellent anti-sag properties, grabs and holds glass, metal and wood in place while the material cures with ambient moisture. It offers high mechanical performance and has excellent resistance to weathering and aging. 4 mm Cut-off, excellent non-sag, available only in black. Cure Type: Moisture
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0424 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Tensile Strength, Ultimate 5.52 - 6.21 MPa
800 - 900 psi
Elongation at Break 550 - 650 %
550 - 650 %
Adhesive Bond Strength 3.79 - 4.17 MPa
550 - 605 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 - 45.0 min
0.500 - 0.750 hour
Tack-free
1440 min
24.0 hour
Value given per 3/16 inches
Shelf Life 9.00 Month
9.00 Month