Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 221 PA66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 221 PA66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benefits: The product offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity. These performances are associated with excellent dimensional stability and good rigidity of molded parts.Available in: Asia Pacific, Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: Connectors, lighters, aerosol valves…Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527 Type 1A
Tensile Stress 30.0 MPa

@Strain 2.50 %
4350 psi

@Strain 2.50 %
40.0 MPa

@Strain 5.00 %
5800 psi

@Strain 5.00 %
45.0 MPa

@Strain 7.50 %
6530 psi

@Strain 7.50 %
50.0 MPa

@Strain 10.0 %
7250 psi

@Strain 10.0 %
60.0 MPa

@Strain 25.0 %
8700 psi

@Strain 25.0 %
Elongation at Break 105 %
105 %
ISO 527 Type 1A
Tensile Modulus 2.00 GPa
290 ksi
ISO 527 Type 1A
Flexural Strength 55.0 MPa
7980 psi
ISO 178
Flexural Modulus 1.40 GPa
203 ksi
ISO 178
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.2
3.2
IEC 60250
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Dissipation Factor 0.080
0.080
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %