| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet |
| Manufacturer | Spartech |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Spartech SP-9013 FR/ABS Flame Retardant Sheet.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 99 | 99 | ASTM D785 |
| Tensile Strength, Yield | 41.4 MPa | 6000 psi | ASTM D638 |
| Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
| Flexural Yield Strength | 67.6 MPa | 9800 psi | ASTM D790 |
| Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
| Izod Impact, Unnotched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D256 |
| 0.587 J/cm @Temperature -40.0 °C |
1.10 ft-lb/in @Temperature -40.0 °F |
ASTM D256 | |
| Falling Dart Impact | 31.2 J | 23.0 ft-lb | 73°F; ASTM D3029 |
| 13.6 J @Temperature -40.0 °C |
10.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 | 5V |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 90 % | 90 % | Gardner; ASTM D2523 |