Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE
Manufacturer Stellarchem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stellarchem GP-975B TPE Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, completely recyclable, colorable & non-hygroscopic thermoplastics elastomer material.Information provided by Stellarchem Polymer & Industrial
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
Particle Mesh Size 80 - 150 Mesh
80 - 150 Mesh
Melt Flow 35.54 g/10 min
35.54 g/10 min
JIS K7210
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
JIS K6301
Tensile Strength, Ultimate 1.96 MPa
284 psi
JIS K6301
Elongation at Break 391 %
391 %
JIS K6301
100% Modulus 0.0196 GPa
2.84 ksi
JIS K6301
300% Modulus 0.00118 GPa
0.171 ksi
JIS K6301
Tear Strength 2.29 kN/m
13.1 pli
JIS K6301-B
Processing Properties Metric English Comments
Processing Temperature 170 - 190 °C
338 - 374 °F
Metering Temperature, Extrusion
Rear Barrel Temperature 150 - 170 °C
302 - 338 °F
Injection Molding
150 - 170 °C
302 - 338 °F
Extrusion
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
160 - 180 °C
320 - 356 °F
Transition, Extrusion
Front Barrel Temperature 170 - 190 °C
338 - 374 °F
Injection Molding
180 - 200 °C
356 - 392 °F
Extrusion
Nozzle Temperature 180 - 200 °C
356 - 392 °F
Injection Molding
Die Temperature 180 - 200 °C
356 - 392 °F
Extrusion
Melt Temperature 150 - 200 °C
302 - 392 °F
Injection Molding
150 - 200 °C
302 - 392 °F
Extrusion
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Injection Molding
Injection Pressure 5.00 - 40.0 MPa
725 - 5800 psi
Injection Molding
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection Molding
Screw Speed 60 - 100 rpm
60 - 100 rpm
Extrusion
100 - 200 rpm
100 - 200 rpm
Injection Molding