| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Carbon Fiber/PTFE Filled |
| Manufacturer | Techmer ES |
| Trade Name | Plaslube® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES Plaslube® J-1/CF/10/TF/20 BK PA66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
| Water Absorption | 1.0 % | 1.0 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 138 MPa | 20000 psi | ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | ASTM D638 |
| Flexural Strength | 207 MPa | 30000 psi | ASTM D790 |
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
| Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | ASTM D648 |
| Surface Resistivity per Square | 10000 ohm - 1e+05 | 10000 ohm - 1e+05 | ASTM D648 |