| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | Unitika |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Unitika A1030TF PA6, Conditioned.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
| Water Absorption | 1.6 % @Time 86400 sec |
1.6 % @Time 24.0 hour |
ISO 62 |
| Moisture Absorption at Equilibrium | 2.5 % | 2.5 % | 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
|
| Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 3.20 mm |
0.018 in/in @Thickness 0.126 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 95 | 95 | ISO 2039 |
| Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527-1/-2 |
| Elongation at Break | 28 % | 28 % | ISO 527-1/-2 |
| Tensile Modulus | 0.840 GPa | 122 ksi | ISO 527-1/-2 |
| Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
| Flexural Modulus | 0.800 GPa | 116 ksi | ISO 178 |
| Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | ISO 179-1 |
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.00e+12 ohm-cm | 7.00e+12 ohm-cm | IEC 60093 |