| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | Unitika |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Unitika A1030TF PA6, Dry.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
| Water Absorption | 1.6 % @Time 86400 sec |
1.6 % @Time 24.0 hour |
ISO 62 |
| Moisture Absorption at Equilibrium | 2.5 % | 2.5 % | 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
|
| Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 3.20 mm |
0.018 in/in @Thickness 0.126 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 116 | 116 | ISO 2039 |
| Tensile Strength, Yield | 68.0 MPa | 9860 psi | ISO 527-1/-2 |
| Elongation at Break | 15 % | 15 % | ISO 527-1/-2 |
| Elongation at Yield | 4.0 % | 4.0 % | ISO 527-1/-2 |
| Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
| Flexural Strength | 90.0 MPa | 13100 psi | ISO 178 |
| Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
| Charpy Impact Unnotched | 8.20 J/cm² | 39.0 ft-lb/in² | ISO 179-1 |
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 120 °C | 248 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.4 @Frequency 1.00e+6 Hz |
3.4 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dissipation Factor | 0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
IEC 60250 |