| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | Unitika |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Unitika M1030B PA6, Dry.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
| Water Absorption | 1.0 % @Time 86400 sec |
1.0 % @Time 24.0 hour |
|
| Moisture Absorption at Equilibrium | 2.8 % | 2.8 % | 50% RH |
| Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.20 mm |
0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.010 cm/cm @Thickness 3.20 mm |
0.010 in/in @Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 113 | 113 | ASTM D785 |
| Tensile Strength at Break | 85.0 MPa | 12300 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Flexural Strength | 133 MPa | 19300 psi | ASTM D790 |
| Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
| Compressive Strength | 85.0 MPa | 12300 psi | ASTM D362 |
| Shear Strength | 62.0 MPa | 8990 psi | ASTM D732 |
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 190 °C | 374 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 120 °C | 248 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
| Dielectric Strength | 27.0 kV/mm | 686 kV/in | ASTM D149 |