Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183-87
Filler Content 50 %
50 %
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 250 MPa
36300 psi
ISO 527-93
Elongation at Break 2.6 %
2.6 %
ISO 527-93
Flexural Strength 355 MPa
51500 psi
ISO 178-93
Flexural Modulus 15.3 GPa
2220 ksi
ISO 178-93
Izod Impact, Notched (ISO) 20.3 kJ/m²
9.66 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ISO 75-93