Physical Properties Metric English Comments
Density 3.70 - 3.80 g/cc
0.134 - 0.137 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9612 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.70 - 3.80 g/cc
0.134 - 0.137 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.76 - 3.80 g/cc
0.136 - 0.137 lb/in³
Sintered
Nabaltec GRANALOX® NM 9622 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Density 3.75 - 3.80 g/cc
0.135 - 0.137 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9622 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.75 - 3.80 g/cc
0.135 - 0.137 lb/in³
Sintered
Nabaltec GRANALOX® NM 9634 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 1.10 - 3.80 g/cc
0.0397 - 0.137 lb/in³
Average value: 1.49 g/cc Grade Count:605
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Density 1.19 - 3.80 g/cc
0.0430 - 0.137 lb/in³
Average value: 1.95 g/cc Grade Count:5
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va..
Density 1.06 - 3.80 g/cc
0.0383 - 0.137 lb/in³
Average value: 1.42 g/cc Grade Count:323
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Density 0.700 - 3.80 g/cc
0.0253 - 0.137 lb/in³
Average value: 1.31 g/cc Grade Count:923
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Density 1.03 - 3.80 g/cc
0.0372 - 0.137 lb/in³
Average value: 1.30 g/cc Grade Count:215
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Density 0.900 - 3.80 g/cc
0.0325 - 0.137 lb/in³
Average value: 1.85 g/cc Grade Count:257
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..
Copyright © lookpolymers.com All Rights Reserved