Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 2781 |
Rogers Corporation Bisco® A2 Sound Barrier Engineered Solid Silicone Mass Layer, Sound Barrier BISCO® A2 Sound Barrier is a solid silicone rubber engineered to meet demanding requirements for flammability, smoke density and toxicity. A2 is used to block the transmission of sound and demonst.. |
|||
Density | 1.64 - 1.65 g/cc | 0.0592 - 0.0596 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 65-2 Linear Low Density Polyethylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Density | 1.64 - 1.65 g/cc | 0.0592 - 0.0596 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 65-4 Polypropylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Density | 1.64 - 1.84 g/cc | 0.0592 - 0.0665 lb/in³ | Average value: 1.71 g/cc Grade Count:30 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Density | 1.64 - 2.10 g/cc | 0.0592 - 0.0759 lb/in³ | Average value: 1.85 g/cc Grade Count:35 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **) Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Celanese ZENITE 6330 LCP, 30% Mineral Reinforced
(Unverified Data**) Zenite® 6330 is a 30% mineral reinforced liquid crystal polymer for injection molding. It has excellent impact resistance, excellent heat deflection temperature and and is well suited for all kinds.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
(Unverified Data**) Fortron 1140L4 is a 40% glass-reinforced grade that is the strongest and toughest product available. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently .. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
(Unverified Data**) Fortron 1140L4 is a 40% glass-reinforced grade that is the strongest and toughest product available. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently .. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Celanese FORTRON 1140L7 PPS, 40% Glass Reinforced
(Unverified Data**) One of the easiest flowing 40% glass reinforced grade in the Fortron product line. This material can be processed at fast cycle times due to the unique crystallization characteristics. This product .. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RX01075 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX01075 is a compound based on Nylon 66 resin containing PTFE, Mineral. Added features of this material include: Heat Stabilized. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KFZ24XXP Acetal Copoly LNP* THERMOCOMP* KFZ24XXP is a compound based on Acetal Copolymer resin containing 20% Glass Fiber, 10% Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled, Inter.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Unitika A1025GO PA6, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Polyplastics Duranex® HN7330 Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR30 NL FY 10 PBT 30% glass fiber reinforced, UL94 V2 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH |
3M AC-236 Class C-20 Aerospace Sealant 3M Aerospace Sealant AC-236 Class C are two-component, manganese dioxide cured, liquid polysulfide polymer systems providing excellent fuel tank and fuselage seals. They have outstanding resistance .. |
|||
Density | 1.64 g/cc @Temperature 23.0 °C |
0.0592 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-201-G30 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.64 g/cc @Temperature 23.0 °C |
0.0592 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-MFC-G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH |
3M AC-236 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Plenco 50335 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |