Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 2781 |
Rogers Corporation Bisco® A2 Sound Barrier Engineered Solid Silicone Mass Layer, Sound Barrier BISCO® A2 Sound Barrier is a solid silicone rubber engineered to meet demanding requirements for flammability, smoke density and toxicity. A2 is used to block the transmission of sound and demonst.. |
|||
Density | 1.64 - 1.65 g/cc | 0.0592 - 0.0596 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 65-3 Polyethylene, 65% Mineral Filled 50% Calcium Carbonate / 15% Titanium Oxide FilledInformation provided by PolyPlastic Group. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Celanese FORTRON 1140L7 PPS, 40% Glass Reinforced
(Unverified Data**) One of the easiest flowing 40% glass reinforced grade in the Fortron product line. This material can be processed at fast cycle times due to the unique crystallization characteristics. This product .. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
LATI Latiohm 80-04 PD01 G/30 PPS, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Density | 1.64 g/cc @Temperature 10.0 °C |
0.0592 lb/in³ @Temperature 50.0 °F |
|
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® SHF4960 PBT Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT LNP THERMOCOMP* WF008 is a compound based on PBT resin containing 40% Glass Fiber. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Unitika A1025GO PA6, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Polyplastics Duranex® HN7330 Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 940 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene Terephthalate Rynite 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength stiffness and low warpage.Informatio.. |
|||
Density | 1.64 - 1.68 g/cc | 0.0592 - 0.0607 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 80/E Flexible PVC, Sheathing Lead Free Under sheathing |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR30 NL FY 10 PBT 30% glass fiber reinforced, UL94 V2 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH |
3M AC-236 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
BASF Heligoen® Blue 6989 F Color Additive Description: Extremely reddish, e-phthalocyanine blue with high chroma and excellent flocculation resistanceChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking.. |
|||
Density | 1.64 g/cc @Temperature 23.0 °C |
0.0592 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-MFC-G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE5264 NC010 PET
(Unverified Data**) Rynite® RE5264 NC010 is a 36% glass fiber reinforced, color stabilized, modified polyethylene terephthalate.Information provided by DuPont Performance Polymers |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America FS-4 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bakelite No.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |