Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.65 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.64 - 1.65 g/cc
0.0592 - 0.0596 lb/in³
ISO 1183
Polyplastic Armoflen® PO MF 65-1 Linear Low Density Polyethylene, 65% Calcium Carbonate
Information provided by PolyPlastic Group.
Density 1.64 - 1.65 g/cc
0.0592 - 0.0596 lb/in³
ISO 1183
Polyplastic Armoflen® PO MF 65-2 Linear Low Density Polyethylene, 65% Calcium Carbonate
Information provided by PolyPlastic Group.
Density 1.64 - 1.65 g/cc
0.0592 - 0.0596 lb/in³
ISO 1183
Polyplastic Armoflen® PO MF 65-3 Polyethylene, 65% Mineral Filled
50% Calcium Carbonate / 15% Titanium Oxide FilledInformation provided by PolyPlastic Group.
Density 1.64 - 1.65 g/cc
0.0592 - 0.0596 lb/in³
ISO 1183
Polyplastic Armoflen® PO MF 65-4 Polypropylene, 65% Calcium Carbonate
Information provided by PolyPlastic Group.
Density 1.20 - 1.65 g/cc
0.0434 - 0.0596 lb/in³
Average value: 1.37 g/cc Grade Count:52
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Density 1.26 - 1.65 g/cc
0.0454 - 0.0596 lb/in³
Average value: 1.33 g/cc Grade Count:74
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Density 1.37 - 1.65 g/cc
0.0495 - 0.0596 lb/in³
Average value: 1.53 g/cc Grade Count:11
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Density 1.39 - 1.65 g/cc
0.0502 - 0.0596 lb/in³
Average value: 1.52 g/cc Grade Count:15
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Density 1.15 - 1.65 g/cc
0.0415 - 0.0596 lb/in³
Average value: 1.33 g/cc Grade Count:36
Overview of materials for PVC, Sheet Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Density 0.549 - 1.65 g/cc
0.0198 - 0.0596 lb/in³
Average value: 1.31 g/cc Grade Count:408
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Density 1.08 - 1.65 g/cc
0.0390 - 0.0596 lb/in³
Average value: 1.32 g/cc Grade Count:14
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Density 1.11 - 1.65 g/cc
0.0401 - 0.0596 lb/in³
Average value: 1.21 g/cc Grade Count:22
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Density 1.61 - 1.65 g/cc
0.0582 - 0.0596 lb/in³
ISO R 1184
Fainplast Compounds RE 337 Rigid PVC, Extrusion
Cheap profiles
Density 1.50 - 1.65 g/cc
0.0542 - 0.0596 lb/in³
Goodfellow Carbon/Vinyl Ester Rod
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Density 1.50 - 1.65 g/cc
0.0542 - 0.0596 lb/in³
Goodfellow Carbon/Vinyl Ester Tube
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Density 1.60 - 1.65 g/cc
0.0578 - 0.0596 lb/in³
Chengdu Polyster RPM450 Flame Retardant Masterbatch
RPM 450 is a red phosphorus based additive flame retardant designed for uses in both glass-fiber reinforced and no-GF reinforced polyamides resins. It is halogen-free and shows more effective flame..
Density 1.22 - 1.65 g/cc
0.0441 - 0.0596 lb/in³
Average value: 1.43 g/cc Grade Count:37
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..
Density 1.33 - 1.65 g/cc
0.0480 - 0.0596 lb/in³
Average value: 1.48 g/cc Grade Count:25
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..
Density 1.26 - 1.65 g/cc
0.0455 - 0.0596 lb/in³
Average value: 1.48 g/cc Grade Count:12
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Density 1.33 - 1.65 g/cc
0.0480 - 0.0596 lb/in³
Average value: 1.42 g/cc Grade Count:31
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Density 1.34 - 1.65 g/cc
0.0484 - 0.0596 lb/in³
Average value: 1.40 g/cc Grade Count:18
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
Density 1.61 - 1.65 g/cc
0.0582 - 0.0596 lb/in³
ISO R 1183
Fainplast Compounds PM 9030 Flexible PVC, Lead Free
Various profiles