Physical Properties Metric English Comments
Density 1.14 - 1.16 g/cc

@Temperature 200 - 215 °C
0.0412 - 0.0419 lb/in³

@Temperature 392 - 419 °F
Average value: 1.15 g/cc Grade Count:6
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Density 1.05 - 1.16 g/cc
0.0379 - 0.0419 lb/in³
Average value: 1.09 g/cc Grade Count:40
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Density 1.00 - 1.16 g/cc
0.0361 - 0.0419 lb/in³
Average value: 1.08 g/cc Grade Count:128
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Density 1.04 - 1.16 g/cc
0.0376 - 0.0419 lb/in³
Apparent
Gouda Vuurvast FI 55-11 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Density 1.10 - 1.16 g/cc
0.0397 - 0.0419 lb/in³
262B Resin
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive
LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum..
Density 1.15 - 1.16 g/cc
0.0415 - 0.0419 lb/in³
Solvay MACKSTAT® DM Surfactant
Product Description: Mackstat DM is a 55% active solution of DMDM Hydantoin, a very effective broad spectrum antimicrobial for cosmetic and personal care products. Due to its high water solubility, ..
Density 1.15 - 1.16 g/cc
0.0416 - 0.0419 lb/in³
ASTM D792
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6)
VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety ..
Density 1.15 - 1.16 g/cc
0.0416 - 0.0419 lb/in³
ASTM D792
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6)
Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of..
Density 1.12 - 1.16 g/cc
0.0405 - 0.0419 lb/in³
ISO R 1183
Fainplast Compounds GS 60/R1 Flexible PVC, Injection Molding for Footwear
Anti-accident soles
Density 1.15 - 1.16 g/cc
0.0416 - 0.0419 lb/in³
ASTM D792
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6)
Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina..
Density 1.15 - 1.16 g/cc
0.0416 - 0.0419 lb/in³
ASTM D792
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6)
Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go..
Density 1.12 - 1.16 g/cc
0.0405 - 0.0419 lb/in³
ISO R 1184
Fainplast Compounds MPH 45/K Medical Flexible PVC, Extrusion
Tubular apparatus
Density 1.12 - 1.16 g/cc
0.0405 - 0.0419 lb/in³
ISO 1183
Austin Novel Materials Texalan® 270A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Density 1.12 - 1.16 g/cc
0.0405 - 0.0419 lb/in³
ISO 1183
Austin Novel Materials Texalan® 470A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.12 - 1.16 g/cc
0.0405 - 0.0419 lb/in³
ISO 1183
Austin Novel Materials Texalan® 670A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.12 - 1.16 g/cc
0.0405 - 0.0419 lb/in³
ISO 1183
Austin Novel Materials Texalan® 370A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech