Nilit FRIANYL B63 KV20 Nylon 6 for injection molding, 20% glass ball reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL B63 KV20 Nylon 6 for injection molding, 20% glass ball reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Water Absorption 1.7 - 2.7 %
1.7 - 2.7 %
ISO 62
Water Absorption at Saturation 6.0 - 8.0 %
6.0 - 8.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.010 - 0.018 cm/cm
0.010 - 0.018 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 150 MPa
21800 psi
ISO 2039-1
Tensile Strength at Break 75.0 MPa
10900 psi
ISO 527
Elongation at Break 11 %
11 %
ISO 527
Tensile Modulus 3.70 GPa
537 ksi
ISO 527
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 3.10 GPa
450 ksi
ISO 178
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
DIN 53453
3.50 J/cm²

@Temperature -40.0 °C
16.7 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
0.600 J/cm²
2.86 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ISO 3146 DSC
Maximum Service Temperature, Air 100 °C
212 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V
550 V
CTI 100; IEC 112