Polyram PlusTek PB350M4 Nylon 6, 20% Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Mineral Filled
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB350M4 Nylon 6, 20% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% mineral filled polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
DIN 53479
Water Absorption 7.2 %
7.2 %
DIN 53495
Moisture Absorption at Equilibrium 2.4 %
2.4 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM-D785
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM-D638
Elongation at Break 4.0 %
4.0 %
ASTM-D638
Flexural Strength 130 MPa
18900 psi
ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
ASTM-D790
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Maximum Service Temperature, Air 70.0 °C
158 °F
Continuous Use
180 °C
356 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4