Material Notes:
Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewable raw materials. ISO polymer designation: PA 10T/X ASTM designation: PPA, polyphthalamide. The main distinguishing features of Grivory HT, when compared to other polyamides, are its good performance at high temperatures. Parts made of Grivory HT provide high stiffness and heat distortion temperatures. Further attributes of Grivory HT are the low moisture absorption, good dimensional stability and excellent chemical resistance.G rivory XE 4065 is especially suitable for parts in the following application areas:Electro / ElectronicsAutomotiveIndustrialSafety equipmentHouseholdInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Water Absorption 1.7 %
1.7 %
ISO 62
Moisture Absorption 0.800 %
0.800 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 245 MPa
35500 psi
dry; ISO 2039-1
245 MPa
35500 psi
conditioned; ISO 2039-1
Tensile Strength at Break 220 MPa
31900 psi
conditioned; ISO 527-1/-2
230 MPa
33400 psi
dry; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
dry; ISO 527-1/-2
2.5 %
2.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 16.0 GPa
2320 ksi
conditioned; ISO 527-1/-2
16.0 GPa
2320 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
conditioned; ISO 179/1eU
9.00 J/cm²
42.8 ft-lb/in²
dry; ISO 179/1eU
8.00 J/cm²

@Temperature 30.0 °C
38.1 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
9.00 J/cm²

@Temperature 30.0 °C
42.8 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
dry; ISO 179/1eA
1.20 J/cm²
5.71 ft-lb/in²
conditioned; ISO 179/1eA
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C
302 °F
long term; EMS
260 °C
500 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 225 °C
437 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
dry; IEC 60093
1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 31.0 kV/mm
787 kV/in
conditioned; IEC 60243-1
32.0 kV/mm
813 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Compressed air systems
Cooling and climate control
Fuel systems
Hydraulic systems
Interior
Powertrain and Chassis
Electricals & Electronics Electrical equipment
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Tools & Accessories
Processing Injection Molding
Product Attributes Bio based Polyamide
Hydrolysis resistant
Improved alcohol resistance
Partially aromatic Polyamide
Special Characteristics Improved heat resistance