Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Laticonther 52/11 GR/70 PP Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LATI
Trade Name Laticonther
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Laticonther 52/11 GR/70 PP Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
Linear Mold Shrinkage, Flow 0.0045 - 0.0080 cm/cm
0.0045 - 0.0080 in/in
Linear Mold Shrinkage, Transverse 0.0045 - 0.0085 cm/cm
0.0045 - 0.0085 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
Elongation at Break 0.60 %
0.60 %
Tensile Modulus 8.20 GPa
1190 ksi
Charpy Impact Unnotched 0.400 J/cm²
1.90 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Thermal Properties Metric English Comments
Thermal Conductivity 15.0 W/m-K
104 BTU-in/hr-ft²-°F
Longitudinal
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
Vicat Softening Point 135 °C

@Load 5.00 kg
275 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 350 ohm-cm
350 ohm-cm
Surface Resistance 85 ohm
85 ohm
Processing Properties Metric English Comments
Melt Temperature 230 - 280 °C
446 - 536 °F
Mold Temperature 50.0 - 80.0 °C
122 - 176 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: