Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0036 - 0.0040 cm/cm @Time 86400 sec |
0.0036 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0036 - 0.0040 cm/cm @Time 86400 sec |
0.0036 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific) LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific) LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific) LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific) LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0035 - 0.0040 cm/cm @Time 86400 sec |
0.0035 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific) LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0035 - 0.0040 cm/cm @Time 86400 sec |
0.0035 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific) LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC LNP* THERMOCOMP* DC006H is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific) LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0035 - 0.0040 cm/cm @Time 86400 sec |
0.0035 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0035 - 0.0040 cm/cm @Time 86400 sec |
0.0035 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific) LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 LNP* STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |