Total PPH 4042 Polypropylene, Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Total Atofina
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 4042 Polypropylene, Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance combined with high clarity, reduced cycle times and good antistatic properties. PPH 4042 is suitable for the injection molding of technical and household items. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ISO 2039-2
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527-2
Elongation at Yield 9.0 %
9.0 %
ISO 527-2
Tensile Modulus 1.65 GPa
239 ksi
ISO 527-2
Flexural Modulus 1.55 GPa
225 ksi
ISO 527-2
Izod Impact, Notched (ISO) 5.50 kJ/m²
2.62 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.650 J/cm²
3.09 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
120°C per hour; ISO 75-2
Vicat Softening Point 90.0 °C
194 °F
50N-50°C per hour; ISO 306
153 °C
307 °F
10N-50°C per hour; ISO 306