Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.10 - 0.20 µm | 0.10 - 0.20 µm | Primary |
NYC YT3CP Y2O3 Powder |
|||
Particle Size | 0.10 µm | 0.10 µm | |
Mallard Creek Polymers ROVENE® 4201 SBR Emulsion ROVENE® 4201 is a carboxylated styrene-butadiene emulsion that has a stiff or "boardy" hand. This binder is recommended for use as a crosslink-able binder for durable nonwovens such as floor main.. |
|||
Particle Size | <= 0.10 µm | <= 0.10 µm | D<sub>50</sub> |
Heraeus Cleviosâ„¢ P VP AI 4083 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP AI 4083 is an antistatic material based o.. |
|||
Particle Size | 0.10 µm | 0.10 µm | SolVin Test |
SolVin 068SA Polyvinyl Chloride Aqueous Dispersion Water-based dispersion of polyvinyl chloride, made by emulsion polymerization. The water-based dispersion (latex) is basic and it is formed
of very fine PVC particles leading to high dispersabilit.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Antimony Nanoparticles General DescriptionAntimony (Sb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Antimony Particles are typically 20-40 nano.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Antimony Oxide Nanopowder General DescriptionAntimony Oxide ( SbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Antimony Tin Oxide Nanoparticles General DescriptionAntimony Tin Oxide (ATO) Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. N.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Barium Titanate nanoparticles General DescriptionBarium Titanate Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nanoscale .. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Bismuth Oxide Nanopowder General DescriptionBismuth Oxide ( BiO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Indium Nanoparticles General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Iron Cobalt Nanopowder General DescriptionIron Cobalt ( FeCo) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Iron Nanoparticles General DescriptionIron (Fe) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Iron Particles are typically 20-40 nanometers (.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Iron Nickel Nanopowder General DescriptionIron Nickel ( FeNi) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nano.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Iron Oxide Nanopowder General DescriptionIron Oxide ( Fe2O3 and Fe3O4) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure part.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Lead Oxide Nanopowder General DescriptionLead Oxide ( PbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Lead Oxide Par.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Manganese Nanoparticles General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Molybdenum Oxide Nanopowder General DescriptionMolybdenum Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles... |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Niobium Oxide Nanoparticles General DescriptionNiobium Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Tantalum Oxide Nanopowder General DescriptionTantalum Oxide ( TaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Tin Oxide Nanopowder General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Tungsten Oxide Nanopowder General DescriptionTungsten Oxide ( WO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide P.. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Calcium Oxide Nanopowder General DescriptionCalcium Oxide ( CaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.10 µm | 0.10 µm | B<sub>4</sub>C Crystal Size |
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |
|||
Particle Size | 0.10 - 0.50 µm | 0.10 - 0.50 µm | SiC Crystal Size |
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |
|||
Particle Size | 0.10 µm | 0.10 µm | Primary; Internal Method |
Solvay Specialty Polymers Algoflon® L100 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L100 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. Algoflon® L100 is specially polymerized to obtain a powder with exceptionally high specific .. |
|||
Particle Size | 0.10 µm | 0.10 µm | |
American Elements Cobalt Iron Nanopowder General DescriptionCobalt Iron ( CoFe) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |