American Elements Barium Titanate nanoparticles

Category Ceramic
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Barium Titanate nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionBarium Titanate Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nanoscale Barium Titanate Particles are typically 20-40 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 7 m 2 /g. Nano Barium Titanate Particles are also available in ultra high purity and high purity and coated and dispersed forms. Applications for Barium Titanate Nanocrystals include for their dielectric properties and in the capacitors for microelectronics and future nano-electronics.
Physical Properties Metric English Comments
Particle Size 0.020 - 0.040 µm
0.020 - 0.040 µm
0.10 µm
0.10 µm
Specific Surface Area 7.0 m²/g
7.0 m²/g
30 - 50 m²/g
30 - 50 m²/g
Molecular Weight 233.21 g/mol
233.21 g/mol