Physical Properties Metric English Comments
Particle Size 160 - 200 µm
160 - 200 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9922 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 5.0 - 200 µm
5.0 - 200 µm
range
Potters Industries Q-Cel® 300
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Particle Size 50 - 200 µm
50 - 200 µm
spherical sizes available
PPT FP110 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Particle Size 50 - 200 µm
50 - 200 µm
spherical sizes available
PPT FP140 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Particle Size 50 - 200 µm
50 - 200 µm
spherical sizes available
PPT FP150 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Particle Size 50 - 200 µm
50 - 200 µm
spherical sizes available
PPT FP160 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Particle Size 50 - 200 µm
50 - 200 µm
spherical sizes available
PPT FP215 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Particle Size 50 - 200 µm
50 - 200 µm
spherical sizes available
PPT FP350 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Particle Size 50 - 200 µm
50 - 200 µm
spherical sizes available
PPT FP500 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Particle Size 50 - 200 µm
50 - 200 µm
spherical sizes available
PPT FP95 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Particle Size 100 - 200 µm
100 - 200 µm
Polimeri Europa Extir® E 5000 AE Expandable Polystyrene  (discontinued **)
Extir E 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or H..
Particle Size 180 - 200 µm
180 - 200 µm
Lucite International Elvacite ® 2010 Acrylic Resin
Elvacite® 2010 is a medium molecular weight methyl methacrylate polymer. 2010 is excellent for use as a general purpose grade for lacquer coatings, such as barrier topcoats for vinyl. It provides..
Particle Size 160 - 200 µm
160 - 200 µm
Lucite International Elvacite ® 2013 Acrylic Resin
Elvacite® 2013 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. It is a fast – dissolving, low viscosity grade with quick solvent release for use in industrial..
Particle Size 120 - 200 µm
120 - 200 µm
Lucite International Elvacite ® 2014 Acrylic Resin
Elvacite® 2014 is a medium molecular weight methyl methacrylate copolymer. 2014 is the softest and most flexible of the Elvacite® copolymer grades. It provides good pigment wetting. ElvaciteÂ..
Particle Size 100 - 200 µm
100 - 200 µm
Lucite International Elvacite ® 4045 Acrylic Resin
Elvacite® 4045 is a medium molecular weight methyl methacrylate polymer. It is designed for use in solvent based screen printing inks, but can be used in a variety of ink formulations.Information..
Particle Size 10 - 200 µm
10 - 200 µm
SPHERE ONE EXTENDOSPHERESâ„¢ PM 6550 Hollow Plastic Spheres
PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide ..
Particle Size 100 - 200 µm
100 - 200 µm
Polimeri Europa Extir® EH 5000 Expandable Polystyrene
Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i..
Particle Size 5.0 - 200 µm
5.0 - 200 µm
range
Potters Industries Q-Cel® 6014
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..