Polymer Property : Particle Size = 50 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 5.0 - 50 µm
5.0 - 50 µm
Potters Industries Sphericel® 45P25 Hollow Engineered Glass Microspheres
Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength..
Particle Size 30 - 50 µm
30 - 50 µm
Mean
Potters Industries Spheriglass® 3000 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Particle Size 40 - 50 µm
40 - 50 µm
Average; for inner type spray system; Microtrac HRA
NYC YT3WBHQ Y2O3 Powder for Spray Coating
High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo c..
Particle Size 5.0 - 50 µm
5.0 - 50 µm
Spherical shape, 5-50 micron distribution. ETM = Equistar Test Method; ETM Malvern
LyondellBasell Microthene® F FA70000 High Density Polyethylene
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
Particle Size 5.0 - 50 µm
5.0 - 50 µm
Spherical shape, 5-50 micron distribution. ETM = Equistar Test Method; ETM Malvern
LyondellBasell Microthene® F FA70900 High Density Polyethylene
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
Particle Size 5.0 - 50 µm
5.0 - 50 µm
Spherical shape, 5-50 micron distribution. ETM = Equistar Test Method; ETM Malvern
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
Particle Size 5.0 - 50 µm
5.0 - 50 µm
Spherical shape, 5-50 micron distribution. ETM = Equistar Test Method; ETM Malvern
LyondellBasell Microthene® F FN50100 Low Density Polyethylene
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
Particle Size 5.0 - 50 µm
5.0 - 50 µm
Spherical shape, 5-50 micron distribution. ETM = Equistar Test Method; ETM Malvern
LyondellBasell Microthene® F FN51000 Low Density Polyethylene
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
Particle Size 5.0 - 50 µm
5.0 - 50 µm
Spherical shape, 5-50 micron distribution. ETM = Equistar Test Method; ETM Malvern
LyondellBasell Microthene® F FN51900 Low Density Polyethylene
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
Particle Size 38 - 50 µm
38 - 50 µm
90%
H.C. Starck Amperit® 584.072 Chromium Carbide-Nickel-Chromium 75-25 (Cr3C2-NiCr)
Particle Size 2.0 - 50 µm
2.0 - 50 µm
PSD (d<sub>50</sub>
Terio Corporation TZOH-40 Zirconium Hydroxide
Information provided by TERIO Corporation.
Particle Size 2.0 - 50 µm
2.0 - 50 µm
PSD (d<sub>50</sub>
Terio Corporation TZOH-50 Zirconium Hydroxide
Information provided by TERIO Corporation.
Particle Size 2.0 - 50 µm
2.0 - 50 µm
PSD (d<sub>50</sub>
Terio Corporation TZOH-60 Zirconium Hydroxide
Information provided by TERIO Corporation.
Particle Size 40 - 50 µm
40 - 50 µm
d90, Guaranteed
TIMCAL TIMREX® C-LUB 310 Primary Synthetic Graphite
Information provided by TIMCAL
Particle Size 30 - 50 µm
30 - 50 µm
D(0.5)
Akzo Nobel Expancel® 551 DE 40 d42 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 30 - 50 µm
30 - 50 µm
D(0.5)
Akzo Nobel Expancel® 551 WE 40 d36 Wet expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 30 - 50 µm
30 - 50 µm
Range (D10 to D90); Laser Diffraction
ALM PA 250 Nylon 12 SLS Prototyping Polymer
Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or..
Particle Size 30 - 50 µm
30 - 50 µm
mean value
Potters Industries Spheriglass® 3000E Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..