Polymer Property : Linear Mold Shrinkage = 0.0310 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0150 - 0.0310 cm/cm
0.0150 - 0.0310 in/in
Average value: 0.0193 cm/cm Grade Count:6
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Linear Mold Shrinkage 0.00200 - 0.0310 cm/cm
0.00200 - 0.0310 in/in
Average value: 0.0134 cm/cm Grade Count:12
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Linear Mold Shrinkage 0.0100 - 0.0310 cm/cm
0.0100 - 0.0310 in/in
Average value: 0.0146 cm/cm Grade Count:41
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..