Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
Polymax® Maxelast® D6975CT TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
Ovation Polymers Nemcon™ E - PP AS Polypropylene, Anti-Static Nemcon™ E-Series products are designed for use in ESDA electronic assembly environments. E PP AS is a moisture independent anti-static polypropylene characterized by consistent moldability and recy.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | |
Resinlab® AR 1018 Conformal Coating Resinlab™ AR 1018 is a one-part low viscosity acrylic based conformal coating for electronic circuit boards. It possesses excellent flexibility and adhesion to many substrates. It provides excell.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | |
LG Chemical SBR 1778 High Acrylonitrile Polymer Description: SBR 1778 is an oil extended cold polymerization SBR with 37.5 parts of discoloring paraffinic/naphthenic oil and light colored high molecular weight styrene-butadiene copolymer of 23.5%.. |
|||
Specific Gravity | 0.920 - 0.940 g/cc | 0.920 - 0.940 g/cc | |
Michelman® Michem® Wood Coating 70M Anionic paraffin blend emulsion Description: Anionic paraffin blend emulsionUsage: Michem® Wood Coating 70M is a high solids, water resistant topical wood treatment for exterior wood and wood composites. It provides good water .. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ISO 2781 |
Kraton® D1160 E (SIS) Linear Triblock Copolymer Description: Kraton D1160 E is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from Europe in the physical form identified: D1160 ES .. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | |
Kraton® D1161 J (SIS) Linear Triblock Copolymer Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D4025 |
Kraton® D4433 P (O/E SIS) Linear Triblock Copolymer Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified:.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ISO 2781 |
Kraton® G1654 E (SEBS) Linear Block Copolymer Kraton G1654 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass.Kraton G1654 ES - supplied as a "fluffy" crumb dusted wit.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-HR-9 TPE Product Description: StarTUFF TF 40-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-9 TPE Product Description: StarTUFF TF 45-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | +/- 0.02; ASTM D792 |
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ CE-505-B Concentrate Based In Polyethylene DescriptionPOLYBATCH® CE-505-B is a specialty masterbatch containing 5% of a slow migrating additive based in polyethylene. This concentrate is designed to reduce film blocking force and COF in LD.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ CE-505-E Concentrate Based In Polyethylene DescriptionPOLYBATCH® CE-505-E is a 5% erucamide slip concentrate based in polyethylene. This concentrate is designed to reduce film COF in LDPE, LLDPE, and mPE cast and blown films. POLYBATCH® .. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ CE-505-B Concentrate Based In Polyethylene DescriptionPOLYBATCH® CE-505-B is a specialty masterbatch containing 5% of a slow migrating additive based in polyethylene. This concentrate is designed to reduce film blocking force and COF in LD.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ISO 1183/1 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Specific Gravity | 0.920 g/cc @Temperature 25.0 °C |
0.920 g/cc @Temperature 77.0 °F |
|
Dow Corning 1503 Fluid A blend of an ultra high viscosity dimethiconol in a low viscosity dimethicone fluid for use in skincare, woundcare, scar therapy, suncare, and color cosmetic applications.Information provided by Do.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | DIN 53479 |
Dynasol Solprene® 1106 Solution Styrene-Butadiene Rubber (SSBR) Solprene® 1106 is a linear high molecular weight random-block styrene/butadiene copolymer with 10% styrene, 6% present as a polystyrene block. This grade has a non-staining antioxidant system; FDA.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
Buckeye Polymers BP FLEX 7000 VPL BLK Thermoplastic Elastomer TPV Product Information: BP Flex TPV's are partially vulcanized thermoplastic elastomers designed to meet higher end applications that require the following performance criteria.Product Features:Higher .. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
Buckeye Polymers BP FLEX 8000 VE BLK Thermoplastic Elastomer TPV Product Information: Our BP Flex 8000 VE Blk material is a general purpose partially crosslinked thermoplastic elastomer using recycled content to achieve maximum economic value and performance for .. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
Aaron Industries AAROLENE® ARPE LD 300-1 LDPE Black Low Density Polyethylene AAROLENE® ARPE 300 Series Polyethylene Compounded Resin, LDPE BlackFeatures: A compounded LDPE, black, low melt resin specifically designed for all profile extrusion applications. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
Asia Technology Pioneers CAP 102 PP Nanocomposite Description: CAP102 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood di.. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | foam molded; ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |
|||
Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
Chase Plastics CP Pryme® PE100-LD2M General Purpose Low Density Polyethylene Information provided by Chase Plastics. |