Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | STN EN ISO 294-4 |
Plastcom PLASTALEN® PH 69 GF 30 Polypropylene reinforced with glass fiber Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm | 0.016 - 0.018 in/in | |
LATI Latene® 11 MDT05-01 PP Homopolymer Polypropylene homopolymer (PPh) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | |
Solvay TECHNYL® PSB 286 PA6, DRY Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm @Thickness 3.20 mm |
0.016 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Thickness 3.18 mm |
0.016 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LH-NBK4/WE1657 Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | DIS 294-4 |
Wellman Wellamid® FR1841-N1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | Eurotec |
Eurotec® Tecodur® PB30 NL PBT, unfilled, natural, high viscosity, extrusion grade Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | Eurotec |
Eurotec® Tecodur® PB70 NL PBT, unfilled, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)
(Unverified Data**) Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | Eurotec |
Eurotec® Tecoform® PO30 GB20 NL HS POM, 20% glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 906 UR POM Copolymer unreinforced, impact modified POM-IInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has .. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Diameter 2.00 mm |
0.016 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a.. |