Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00800 - 0.00900 cm/cm | 0.00800 - 0.00900 in/in | Average value: 0.00867 cm/cm Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0400 cm/cm | 0.00800 - 0.0400 in/in | Average value: 0.0140 cm/cm Grade Count:25 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0156 cm/cm | 0.00800 - 0.0156 in/in | Average value: 0.0113 cm/cm Grade Count:5 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.00900 cm/cm | 0.00800 - 0.00900 in/in | Average value: 0.00833 cm/cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0300 cm/cm | 0.00800 - 0.0300 in/in | Average value: 0.0226 cm/cm Grade Count:6 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0302 cm/cm | 0.00800 - 0.0302 in/in | Average value: 0.0171 cm/cm Grade Count:78 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0120 cm/cm | 0.00800 - 0.0120 in/in | Average value: 0.0104 cm/cm Grade Count:5 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0230 cm/cm | 0.00800 - 0.0230 in/in | Average value: 0.0148 cm/cm Grade Count:3 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0100 cm/cm @Temperature 80.0 - 80.0 °C |
0.00800 - 0.0100 in/in @Temperature 176 - 176 °F |
Average value: 0.00867 cm/cm Grade Count:3 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0200 cm/cm | 0.00800 - 0.0200 in/in | Average value: 0.0169 cm/cm Grade Count:15 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0110 cm/cm | 0.00800 - 0.0110 in/in | Average value: 0.00958 cm/cm Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |