Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | ASTM D955 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO 294-4 |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm @Thickness 3.18 mm |
0.011 - 0.013 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® PS-30CF/000 HF UV BLACK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | |
LATI Larpeek 10 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Latilub 52/30-15T G/30 PP Homopolymer, 30% Glass Fiber Reinforced Self-lubricating product based on Polypropylene homopolymer (PPh). PTFE. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0095 - 0.013 cm/cm | 0.0095 - 0.013 in/in | |
LATI Latilub 62-15ST PA6 Self-lubricating product based on Polyamide 6 (PA6). Silicone / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm @Thickness 3.18 mm |
0.011 - 0.013 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm @Thickness 0.750 - 2.30 mm |
0.0090 - 0.013 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm @Time 86400 sec |
0.011 - 0.013 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07435 LNP* THERMOCOMP* is a compound based on Miscellaneous resin containing Proprietary Filler(s). Added feature of this grade is: Plateable. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm @Time 86400 sec |
0.0090 - 0.013 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Asia Pacific) Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.013 cm/cm @Thickness 3.20 mm |
0.0080 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA (Asia Pacific) High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PS+PA High flow PPE+PS+PA for under-the-hood and electrical applications. With mold release |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF33-66 XE-BKDX9 33% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | DIS 294-4 |
Wellman Wellamid® GF33A099-HRBK Nylon 66, 33% Glass Fiber Reinforced, Hydrolysis Resistant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1599-N Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm @Time 86400 sec |
0.0090 - 0.013 in/in @Time 24.0 hour |
ISO 294 |
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Asahi Kasei Method |
Asahi Kasei Tenac® GA510 Homopolymer Acetal Resin 10% Glass fiber filled grade with high stiffness and superior dimensional stability.Information provided by Asahi Kasei Corporation. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | ASTM D955 |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Latimass 52/35-04 D009 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.013 cm/cm | 0.0105 - 0.013 in/in | |
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | |
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |