Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.500 - 0.680 g/cc | 0.0181 - 0.0246 lb/in³ | Average value: 0.586 g/cc Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Apparent Bulk Density | 0.600 - 0.680 g/cc | 0.0217 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Apparent Bulk Density | 0.620 - 0.680 g/cc | 0.0224 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Apparent Bulk Density | 0.620 - 0.680 g/cc | 0.0224 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Apparent Bulk Density | 0.620 - 0.680 g/cc | 0.0224 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |
|||
Apparent Bulk Density | 0.600 - 0.680 g/cc | 0.0217 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |