Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.100 - 84.0 g/10 min | 0.100 - 84.0 g/10 min | Average value: 15.8 g/10 min Grade Count:70 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Melt Flow | 0.100 - 96.0 g/10 min | 0.100 - 96.0 g/10 min | Average value: 20.7 g/10 min Grade Count:28 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melt Flow | 0.100 - 42.0 g/10 min | 0.100 - 42.0 g/10 min | Average value: 9.51 g/10 min Grade Count:177 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Melt Flow | 0.100 - 35.0 g/10 min | 0.100 - 35.0 g/10 min | Average value: 4.93 g/10 min Grade Count:103 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Melt Flow | 0.100 - 42.0 g/10 min | 0.100 - 42.0 g/10 min | Average value: 7.62 g/10 min Grade Count:26 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Flow | 0.100 - 17.0 g/10 min | 0.100 - 17.0 g/10 min | Average value: 6.10 g/10 min Grade Count:34 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Flow | 0.100 - 10.0 g/10 min | 0.100 - 10.0 g/10 min | Average value: 3.44 g/10 min Grade Count:20 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Flow | 0.100 - 12.0 g/10 min | 0.100 - 12.0 g/10 min | Average value: 3.08 g/10 min Grade Count:18 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Melt Flow | 0.100 - 23.6 g/10 min | 0.100 - 23.6 g/10 min | Average value: 4.69 g/10 min Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma.. |
|||
Melt Flow | 0.100 - 60.0 g/10 min | 0.100 - 60.0 g/10 min | Average value: 15.7 g/10 min Grade Count:39 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Melt Flow | 0.100 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 0.100 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-6045 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 0.100 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-6055 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 0.100 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-6065 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 0.100 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-6075 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 0.100 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-6085 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |