Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.700 - 53.5 g/10 min | 0.700 - 53.5 g/10 min | Average value: 18.2 g/10 min Grade Count:66 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Melt Flow | 0.700 - 230 g/10 min | 0.700 - 230 g/10 min | Average value: 13.1 g/10 min Grade Count:106 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Melt Flow | 0.700 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.700 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2327-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 0.700 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.700 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-86-K975-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 0.700 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.700 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-88-N809C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 0.700 - 110 g/10 min | 0.700 - 110 g/10 min | Average value: 32.7 g/10 min Grade Count:15 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Melt Flow | 0.700 - 20.0 g/10 min | 0.700 - 20.0 g/10 min | Average value: 2.83 g/10 min Grade Count:46 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Melt Flow | 0.700 - 14.0 g/10 min | 0.700 - 14.0 g/10 min | Average value: 3.43 g/10 min Grade Count:27 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Melt Flow | 0.700 - 16.0 g/10 min | 0.700 - 16.0 g/10 min | Average value: 4.18 g/10 min Grade Count:124 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Melt Flow | 0.700 - 40.0 g/10 min | 0.700 - 40.0 g/10 min | Average value: 10.7 g/10 min Grade Count:131 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |