SABIC Innovative Plastics NORYL WCD825 PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCD825 PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible, very low-migration, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-1 requirement. 80C temperature rating and excellent heat deformation performance as defined by UL 1581. 82 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Melt Flow 3.2 g/10 min

@Load 5.00 kg,
Temperature 250 °C
3.2 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
30S reading; ASTM D2240
Tensile Strength at Break 15.0 MPa
2180 psi
50 mm/min; ISO 527
16.0 MPa
2320 psi
Type I, 50 mm/min; ASTM D638
20.0 MPa
2900 psi
after 7days @113°C; UL 1581
21.0 MPa
3050 psi
UL 1581
Elongation at Break 190 %
190 %
after 7days @113°C; UL 1581
203 %
203 %
50 mm/min; ISO 527
220 %
220 %
Type I, 50 mm/min; ASTM D638
245 %
245 %
UL 1581
Flexural Modulus 0.0200 GPa
2.90 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.0200 GPa
2.90 ksi
12.5 mm/min; ISO 178
Heat Distortion 7.0 %

@Load 0.250 kg,
Temperature 100 °C
7.0 %

@Load 0.551 lb,
Temperature 212 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
UL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Oxygen Index 25 %
25 %
ISO 4589
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 5.80e+15 ohm-cm
5.80e+15 ohm-cm
ASTM D257
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm

@Thickness 2.00 mm
635 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0030

@Frequency 1.00e+6 Hz
0.0030

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 110
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 60
ASTM E 662
VW-1 Pass
UL 1581